1mm thick:
name of the paint |
paintingarea/kg |
used amount/㎡ |
thickness(about) |
epoxy sealing primer |
6㎡/kg |
0.17 kg/㎡ |
15um |
epoxy floor intermediate coat paint |
1㎡/kg
(with sand) |
1
kg/㎡ |
0.3 kg/㎡ |
540um |
quartz sand |
0.7kg/㎡ |
lay the conductive copper foil |
------ |
------ |
------ |
epoxy conductive intermediate coat paint |
2㎡/kg |
0.5 kg/㎡ |
300um |
antistatic floor topcoat |
2.5㎡/kg(twice) |
0.4 kg/㎡ |
160um |
diluent |
------ |
------ |
------ |
2mm thick:
name of the paint |
paintingarea/kg |
used amount/㎡ |
thickness(about) |
epoxy sealing primer |
6㎡/kg |
0.17 kg/㎡ |
15um |
epoxy floor intermediate coat paint |
0.4㎡/kg
(with sand) |
2.5
kg/㎡ |
0.75 kg/㎡ |
1540um |
quartz sand |
1.75 kg/㎡ |
lay the conductive copper foil |
------ |
------ |
------ |
epoxy conductive intermediate coat paint |
2㎡/kg |
0.5 kg/㎡ |
300um |
antistatic floor topcoat |
2.5㎡/kg(twice) |
0.4 kg/㎡ |
160um |
diluent |
1/5of the amount of the paint |
------ |
3mm thick:
name of the paint |
paintingarea/kg |
used amount/㎡ |
thickness(about) |
epoxy sealing primer |
6㎡/kg |
0.17 kg/㎡ |
15um |
epoxy floor intermediate coat paint |
0.28㎡/kg
(with sand) |
3.6
kg/㎡ |
1.1 kg/㎡ |
2540um |
quartz sand |
2.5 kg/㎡ |
conductive copper foil |
------ |
------ |
------ |
epoxy conductive intermediate coat paint |
2㎡/kg |
0.5 kg/㎡ |
300um |
antistatic floor topcoat |
2.5㎡/kg(twice) |
0.4 kg/㎡ |
160um |
diluent |
1/5of the amount of the paint |
------ |
construction reference:
1. substrate treatment: the temperature is above 5℃. the relative humidity is less than 75%. the new cement floor can be painted after being dried for 28 days. remove the dirt and repair the old and loose place. wear the surface with electric buffing machine. remove the dust. ensure that no dust, no water, no grease.
2. paint the epoxy sealing primer: mix the two compents of the epoxy sealing primer according to the proportion and stir it. after laying the paint for 10 minutes roller coat the paint.(use it up within 6 hours or it will become blue). after 12 hours paint next layer.
3. paint intermediate coat mortar: wear it after at least 12 hours when the primer is dry. mix the two compents according to the proportion and stir it. after 10 minutes mix the paint and quartz sand according to the proportion of 3︰7 and stir it .the mortar can be used.( use it up within 6hours or it will become blue), wear and clean the surface after a day of drying.
4. lay the conductive copper foil: lay the conductive copper foil(2m*6m grid)connecting with earthing terminal.
5. brush the conductive intermediate coat: mix the intermediate coat paint according to the proportion and leave it alone for 10 minutes and scrape it with trowel. wear the surface after 24h of drying. then the next work can be done.
6. paint the topcoat: mix the two components of topcoat according to the proportion and leave it alone for 10 minutes. roller coat it with special rolling brush. after 24h paint second layer of topcoat with special rolling brush. after 48h staffs are allowed in. use it after 7 days of maintenance.
|